ALFAPOL EP-1P — epoxy impregnation for concrete floors
Two-component epoxy impregnation that protects concrete from aggressive chemicals, eliminates dusting and hardens the surface.

The PU-4VN ASKh polymer-concrete coating combines antistatic properties with chemical resistance, water resistance and heat resistance — up to +130 °C depending on the version. The surface can be smooth or textured rough, in a muted tinted shade. Shore D hardness is at least 80, compressive strength 40 MPa, flexural strength 12 MPa, electrical resistance below 10⁶ Ω; full load after 7 days.
| Manufacturer | ALFAPOL — OOO “ALFAPOL”, Saint Petersburg |
|---|---|
| Type | polyurethane-cement floors |
| Use | production halls, warehouses and logistics, food and pharmaceutical, chemically resistant, antistatic/conductive, wet areas, outdoor areas |
| Base | polyurethane-cement; Polyurethane-cement antistatic chemical-resistant and heat-resistant floor |
| Colour | The tinted polymer-concrete coating has a smooth or textured rough surface in a muted shade |
| Packaging | Plastic containers: Component A 3.5 kg, Component B 3.0 kg. Polypropylene bag: Component C 25 kg |
| Application temperature | Application temperature, °C: +10°C to +30°C |
| Curing | At 20 °C: foot traffic after 3 days, medium load after 5 days, full load after 7 days; Recoat interval, h, min.: 24; Foot traffic, h, min.: 72; Full cure, days, min.: 7 |
| Key properties | Service temperature, °C: 6 mm layer -25 to +80, 9 mm layer -40 to +120, 12 mm layer -40 to +130; Shore D hardness, min.: 80; Compressive strength, MPa: 40; Flexural tensile strength, MPa: 12; Bond strength to concrete (failure in concrete), min., MPa: 2.0; Surface electrical resistance, Ohm, less than: 10^6; Volume electrical resistance, less than: 10^6 |
| Layer thickness | Layer thickness, mm: 5-15 |
| Consumption | at 5 mm layer thickness – 10 kg/m². |
| Shelf life | Shelf life, months: 6 |
| Standards | TU 23.64.10-006-82166262-2018 |
Data from the manufacturer’s technical data sheet. The coating system, number of coats and quantity are selected for your project on request.
Two-component epoxy impregnation that protects concrete from aggressive chemicals, eliminates dusting and hardens the surface.
Non-sparking concrete floor laid at temperatures from −5 to +10 °C, for workshops, warehouses and open areas.
Magnesite-based barite concrete for radiation-shielding floor screeds, used together with ShT-BARIT plaster for walls and ceilings.
Two-component epoxy primer for mineral substrates before polymer coatings and a base for quartz-filled putty.
Heat-resistant floor coating on high-alumina cement with crushed chamotte for forging, steelmaking and heat-treatment facilities.
Protective curing impregnation for concrete that prevents surface defects caused by rapid water evaporation during hardening.