LEVELINE FC70 S quartz dry-shake topping — hardening fresh concrete floors
Dry quartz mix for hardening freshly laid concrete in workshops, warehouses and car parks; compressive strength from 70 MPa at 28 days.

The finishing mortar Profskrin RC40 Sm, based on Portland cement, sand up to 0.63 mm and fibre, reaches at least 20 MPa in compression after 24 hours, 30 MPa after 7 days and 40 MPa after 28 days, with flexural strength from 6 MPa. It is used for structural repair of load-bearing building and bridge structures, treatment and industrial facilities, underground ducts and pipelines. The mix retains workability for 60 minutes, bond to the substrate is from 1.5 MPa, frost resistance at least 300 cycles.
| Manufacturer | INDASTRO — OOO Sedrus |
|---|---|
| Type | thixotropic repair mortars |
| Use | bridges and overpasses, tanks and treatment plants, industrial buildings, columns and beams |
| Base | Portland cement, graded sand with particle size up to 0.63 mm, fibre, modifying admixtures |
| Packaging | bags 25 kg |
| Application method | Profskrin RC40 Sm finishing repair mortar is used for structural repair of concrete structures: Load-bearing building structures; Bridge structures; Treatment facilities; Underground engineering structures; Industrial structures |
| Application temperature | +5…+30 °C |
| Key properties | mixing water: 0.16-0.17; compressive strength at 24 h: ≥20 MPa; compressive strength at 7 days: ≥30 MPa; compressive strength at 28 days: ≥40 MPa; flexural strength at 28 days: ≥6 MPa; bond strength to substrate: ≥1.5 MPa; workability retention: 60 min; frost resistance: ≥300 cycles; maximum aggregate size, mm: 0.63 |
| Shelf life | 12 months in the original factory packaging from the date of manufacture, in a dry room |
Data from the manufacturer’s technical data sheet. The coating system, number of coats and quantity are selected for your project on request.
Dry quartz mix for hardening freshly laid concrete in workshops, warehouses and car parks; compressive strength from 70 MPa at 28 days.
Winter version of the thixotropic R4 mortar for repairing B30–B40 concrete at temperatures from −10 to +10 °C; compressive strength at 28 days from 45 MPa.
Cementitious grout for installing equipment, columns, joints and anchors at low temperatures; 10 MPa after 6 hours at −10 °C, 50 MPa at 28 days.
Thixotropic R4 mortar for repairing high-strength concrete and reinforced concrete of B50 and above; 70 MPa at 28 days, water impermeability W20.
Cementitious compound for protecting reinforcement against corrosion and forming a bonding layer in concrete repair; bond to the substrate from 2.0 MPa.
Clear polyurethane sealer for curing freshly laid concrete and toppings in workshops and warehouses; dries in 2 hours at +20 °C.