LEVL Coat 070 — catalyst for LEVL methyl methacrylate floors
Powder polymerisation catalyst for LEVL Coat 171, 271 and 573 carboacrylate materials; the dosage depends on temperature.

A damaged area of a floor with a hardened top layer is restored with the same LEVL Top topping, gauged with LEVL RemTop. First, a primer is prepared from RemTop and water and applied by brush or roller; then it is mixed with the topping and the repair mix is laid wet-on-wet, finishing with LEVL Cure 100 curing. Bond strength to the substrate is at least 1.5 MPa, and the repaired areas are not inferior to the topping in strength. Supplied in a 1.25 kg plastic pail; the compound is not acid-resistant.
| Manufacturer | LEVL (INGRI) — OOO “Ingri”, Saint Petersburg |
|---|---|
| Type | concrete floor repair |
| Use | production workshops, warehouses and logistics |
| Base | dry polymer-cement mix (primer and gauging agent for LEVL Top topping) |
| Packaging | plastic pail with lid, 1.25 kg |
| Application method | local repair of topping floors: primer (2.5 kg of water per 1.25 kg of RemTop) by brush/roller, then the repair mix of 3.75 kg of the priming solution per 25 kg of LEVL Top, wet-on-wet; curing with LEVL Cure 100 |
| Application temperature | +5…+30 °C (ambient and substrate); concrete at least B22.5; 3 days without draughts |
| Key properties | Bond strength to substrate at least 1.5 MPa; grain size 0.16 mm; strength of repaired areas “not inferior to the topping”; not acid-resistant |
| Layer thickness | system example: 10 mm |
| Consumption | priming 0.1 kg/m² (+ water 0.2 kg/m²); main layer 10 mm: RemTop 1.08 kg/m² + LEVL Top 21.6 kg/m² + water 2.16 kg/m² |
| Shelf life | 12 months; storage at +5…+30 °C |
| Standards | TU 5745-025-94613022-10 with Amendment No. 1; GOST 31356; not subject to fire safety certification (Decision No. 00134R-05/13) |
Data from the manufacturer’s technical data sheet. The coating system, number of coats and quantity are selected for your project on request.
Powder polymerisation catalyst for LEVL Coat 171, 271 and 573 carboacrylate materials; the dosage depends on temperature.
Two-component epoxy impregnation for dustproofing and hardening porous mineral substrates; adhesion to concrete over 4.0 MPa.
Highly elastic thermoplastic polyolefin tape on epoxy adhesive for expansion joints, cold joints and moving cracks; elongation 600%.
Self-levelling mix for preparing concrete for polymer and cementitious coatings in workshops and warehouses; flexural strength 8 MPa.
Smooth seamless epoxy coating for nuclear industry rooms subject to decontamination; Shore D hardness at least 70.
Two-component semi-gloss RAL paint coating for workshops, car parks, food production and schools; Taber abrasion up to 65 mg.